Regulacje i polityka gospodarcza · 22/12/2005
U.S. Imposes Antidumping Duty on Japanese Superalloy Degassed Chromium
The U.S. Department of Commerce has issued an antidumping duty order on superalloy degassed chromium imports from Japan, following affirmative final determinations by the Department of Commerce and International Trade Commission.